Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 76.0 - 270 °C | 169 - 518 °F | Average value: 92.7 °C Grade Count:16 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |