Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 11.0 °C @Load 5.10 kg |
51.8 °F @Load 11.2 lb |
Rate A (50°C/h); ASTM D1525 |
Styron PULSEâ„¢ EXT 200 PC/ABS Engineering Resin Overview: High Heat, High Impact PC/ABS resin for injection molded automotive plating and painting trim applications.Information provided by Styron |