Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 259 °C | 498 °F | ASTM D1525 |
PlastxWorld CEVIAN® S1500 High Heat PC/ABS alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |