Vicat Softening Point 95.0 - 240 °C
203 - 464 °F
Average value: 113 °C Grade Count:16
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
Vicat Softening Point 215 - 240 °C
419 - 464 °F
Average value: 235 °C Grade Count:5
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..