Polymer Property : Vicat Softening Point = 46.7 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 46.7 °C
116 °F
ASTM D1525
ExxonMobil Escorene™ UL 00226CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00226CC is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperature above 230°C (446°F) may cause resin degradation.Availability: Africa & Mi..
Vicat Softening Point 46.7 °C
116 °F
ASTM D1525
ExxonMobil Escorene™ FL 00226CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00226CC is a copolymer of ethylene and vinyl acetate offering low gel. Processing Conditions: Processing temperatures above 230°C (446°F) may cause resin degradation. Machi..