Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 237 °C | 459 °F | B |
Plastcom SLOVAMID 66 LI PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Vicat Softening Point | 237 °C | 459 °F | B |
Plastcom SLOVAMID 66 LI TS PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Vicat Softening Point | 237 °C | 459 °F | B/50; ISO 306 |
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 237 °C @Load 5.10 kg |
459 °F @Load 11.2 lb |
ISO 306 |
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro.. |
|||
Vicat Softening Point | 237 °C @Load 5.10 kg |
459 °F @Load 11.2 lb |
ISO 306 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Vicat Softening Point | 237 °C | 459 °F | 50N; ISO 306 |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Vicat Softening Point | 237 °C @Load 5.10 kg |
459 °F @Load 11.2 lb |
ISO 306 |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |