Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 52.0 - 192 °C | 126 - 378 °F | Average value: 110 °C Grade Count:62 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |