Polymer Property : Vicat Softening Point = 36.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 36.0 - 150 °C
96.8 - 302 °F
Average value: 89.8 °C Grade Count:20
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Vicat Softening Point 36.0 °C
96.8 °F
ASTM D1525, ISO 306
DuPont Elvax® 150 Ethylene Vinyl Acetate
DuPont™ Elvax® 150 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 150 resins can be used for the following applications: molding, compoundin..
Vicat Softening Point 36.0 °C
96.8 °F
ASTM D1525, ISO 306
DuPont Elvax® 150W Ethylene Vinyl Acetate
DuPont™ Elvax® 150W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p..
Vicat Softening Point 36.0 °C
96.8 °F
B (50N); ISO 306
Borealis Daplen™ KB4436 TPO Compound
Daplen KB4436 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen KB4436 is a material with excellent impact/stiffness ratio. Thanks to its low the..
Vicat Softening Point 36.0 °C
96.8 °F
ASTM D1525, ISO 306
DuPont Elvax® 150W-LG Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 150W-LG is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent th..
Vicat Softening Point 36.0 - 161 °C
96.8 - 322 °F
Average value: 111 °C Grade Count:110
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..