Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 145 - 154 °C | 293 - 310 °F | Average value: 152 °C Grade Count:4 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |