Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 40.0 - 153 °C | 104 - 307 °F | Average value: 63.7 °C Grade Count:20 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |