Polymer Property : Vicat Softening Point = 242 °F
Polymer Property :
Vicat Softening Point =
242 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Vicat Softening Point
117
°C
242
°F
0.125 inch, 1 Kg; ASTM D1525
Diamond Polymers ABS TM 25
Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc.