Polymer Property : Vicat Softening Point = 241 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 - 116 °C
194 - 241 °F
Average value: 104 °C Grade Count:5
Overview of materials for Polybutene
This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..