Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 236.4 °C | 457.5 °F | ISO 306 |
Tisan TISAPET® 30% Glass Reinforced Polyethylene Terephthalate Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a.. |