Polymer Property : Vicat Softening Point = 209 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 98.3 °C
209 °F
ASTM D1525
Total 620 Polystyrene  (discontinued **)
Polystyrene 620 is an impact polystyrene designed for high gloss cap layers. The polymer has been specifically designed for co extrusion processing to produce a ductile sheet with an extremely high ..
Vicat Softening Point 98.3 °C
209 °F
ASTM D1525
Ravago Manufacturing Americas Hylac® GP48 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Vicat Softening Point 98.3 °C

@Load 1.02 kg
209 °F

@Load 2.25 lb
120°C/h; ASTM D 1525
Styrolution PS 3600/3601 GPPS
Exceptional flow characteristicsGood for thin wall and complex partsUSP Class VI certifiedInformation provided by Styrolution
Vicat Softening Point 98.3 °C
209 °F
ASTM D1525
American Polymers API 390 Polystyrene
API 390 is a general purpose polystyrene produced in pellet form for injection molding. API 390 has excellent clarity and easy flow.Applications: Used in the manufacture of cosmetic containers, hou..
Vicat Softening Point 98.3 °C
209 °F
ASTM D1525
Total PSI 960E Polystyrene
Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids ..
Vicat Softening Point 98.3 °C
209 °F
Rate A (50°C/h), Loading 1 (10 N); ASTM D1525
Entec Hyrene® PSCRY 14 General Purpose Polystyrene
Available in North America Features: General PurposeRoHS Compliant Form: Pellets Information provided by Entec
Vicat Softening Point 98.3 °C
209 °F
ASTM D648
Amco Amalloy® B1044 Polymer Alloy
Amco Amalloy B1044 is a proprietary copolymer with exceptional clarity and toughness.Low haze, low melt flow, high tensile & flexural strength.Information provided by Amco Plastic Materials.