Thermal Properties Metric English Comments
Vicat Softening Point 178.1 °C
352.6 °F
10 N; ASTM D1252
CRP Technology Windform® XT Polyamide-Carbon Composite
WindForm™ XT Composite is a new generation material, in which the mechanical characteristics are excellent for Rapid Manufacturing. Black coloured compound polyamide and carbon based material with ..