Polymer Property : Vicat Softening Point = 176.1 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 176.1 °C
349.0 °F
10 N; ISO 306 TYPE A50
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
Processed by selective laser sintering (SLS). Windform® XT 2.0 is the evolution of the ground breaking high performance Windform® XT, the carbon fiber reinforced composite material, known for its..