Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 63.0 - 65.0 °C @Load 5.00 kg |
145 - 149 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RST 0413 Rigid PVC, Extrusion Lead Free Transparent antishock profiles |