Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 87.0 - 148 °C | 189 - 298 °F | Average value: 117 °C Grade Count:3 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |