Polymer Property : Vicat Softening Point = 108 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 75.0 - 108 °C
167 - 226 °F
Average value: 95.5 °C Grade Count:98
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Vicat Softening Point 82.8 - 108 °C
181 - 226 °F
Average value: 97.7 °C Grade Count:72
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..