Polymer Property : Vicat Softening Point = 100.5 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 100.5 °C
212.9 °F
ASTM D1525
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene
SV - 0157 ABS extrusion grade has been formulated to provide excellent mechanical properties, extrusion stability, vacuum formability and chemical resistance. It has low flow with high impact streng..
Vicat Softening Point 100.5 °C
212.9 °F
50°C/hr, 50N; ISO 306-B50
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS)
MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun ..
Vicat Softening Point 100.5 °C
212.9 °F
0.125 inch, 1 Kg; ASTM D1525
Diamond Polymers ABS VP-11 ELG
Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc.