Shear Modulus 0.6221 GPa

@Temperature 60.0 °C
90.23 ksi

@Temperature 140 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani..
Shear Modulus 0.6221 GPa

@Temperature 60.0 °C
90.23 ksi

@Temperature 140 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b..