Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 59.3 GPa @Temperature 50.0 °C |
8600 ksi @Temperature 122 °F |
|
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |