Mechanical Properties Metric English Comments
Shear Modulus 57.0 GPa

@Temperature 900 °C
8270 ksi

@Temperature 1650 °F
Dynamic
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 57.0 GPa

@Temperature 900 °C
8270 ksi

@Temperature 1650 °F
Dynamic
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 57.0 GPa

@Temperature 900 °C
8270 ksi

@Temperature 1650 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 57.0 GPa

@Temperature 900 °C
8270 ksi

@Temperature 1650 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 57.0 GPa

@Temperature 900 °C
8270 ksi

@Temperature 1650 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 57.0 GPa

@Temperature 900 °C
8270 ksi

@Temperature 1650 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 57.0 GPa

@Temperature 900 °C
8270 ksi

@Temperature 1650 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 57.0 GPa

@Temperature 871 °C
8270 ksi

@Temperature 1600 °F
ATI Allegheny Ludlum AL 625HP™ Stainless Steel
Nickel-based superalloy. Characteristics:exceptional fatigue resistance, excellent resistance to oxidation and corrosion, outstanding strength and toughness over a range of temperatures from cryogen..
Shear Modulus 57.0 GPa

@Temperature 900 °C
8270 ksi

@Temperature 1650 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Shear Modulus 57.0 GPa

@Temperature 900 °C
8270 ksi

@Temperature 1650 °F
Dynamic
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Shear Modulus 57.0 GPa

@Temperature 649 °C
8270 ksi

@Temperature 1200 °F
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel
INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-..