Mechanical Properties Metric English Comments
Shear Modulus 65.0 GPa

@Temperature 700 °C
9430 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 65.0 GPa

@Temperature 700 °C
9430 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 65.0 GPa

@Temperature 700 °C
9430 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 65.0 GPa

@Temperature 700 °C
9430 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 65.0 GPa

@Temperature 700 °C
9430 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 65.0 GPa

@Temperature 700 °C
9430 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 65.0 GPa

@Temperature 316 °C
9430 ksi

@Temperature 601 °F
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy
The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt..
Shear Modulus 65.0 GPa

@Temperature 700 °C
9430 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Shear Modulus 65.0 GPa

@Temperature 700 °C
9430 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..