Mechanical Properties Metric English Comments
Shear Modulus 61.0 GPa

@Temperature 843 °C
8850 ksi

@Temperature 1550 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Shear Modulus 61.0 GPa

@Temperature 843 °C
8850 ksi

@Temperature 1550 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Shear Modulus 61.0 GPa

@Temperature 843 °C
8850 ksi

@Temperature 1550 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1121°C, air cooled, aged 16 hours at 899°C
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Shear Modulus 61.0 GPa

@Temperature 800 °C
8850 ksi

@Temperature 1470 °F
Dynamic
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 61.0 GPa

@Temperature 800 °C
8850 ksi

@Temperature 1470 °F
Dynamic
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 61.0 GPa

@Temperature 800 °C
8850 ksi

@Temperature 1470 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 61.0 GPa

@Temperature 800 °C
8850 ksi

@Temperature 1470 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 61.0 GPa

@Temperature 800 °C
8850 ksi

@Temperature 1470 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 61.0 GPa

@Temperature 800 °C
8850 ksi

@Temperature 1470 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Shear Modulus 61.0 GPa

@Temperature 800 °C
8850 ksi

@Temperature 1470 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Shear Modulus 61.0 GPa

@Temperature 843 °C
8850 ksi

@Temperature 1550 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include ..
Shear Modulus 61.0 GPa

@Temperature 800 °C
8850 ksi

@Temperature 1470 °F
Dynamic
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..