Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 4.00 GPa @Temperature 0.000 °C |
580 ksi @Temperature 32.0 °F |
|
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Shear Modulus | 4.00 GPa @Temperature 0.000 °C |
580 ksi @Temperature 32.0 °F |
|
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Shear Modulus | 4.00 GPa @Temperature 0.000 °C |
580 ksi @Temperature 32.0 °F |
|
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |