Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.90 GPa @Temperature 149 °C |
421 ksi @Temperature 300 °F |
In-Plane; Wet |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber Information provided by HexCel |