Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 4.62 GPa @Temperature 23.9 °C |
670 ksi @Temperature 75.0 °F |
In-Plane, Dry, 365° Oven Cured; ASTM D3518 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 12K PW HTS Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |