Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 4.27 GPa @Temperature 23.0 °C |
619 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber Information provided by HexCel |