Polymer Property : Shear Modulus = 4.14 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 4.14 GPa

@Temperature 121 °C
600 ksi

@Temperature 250 °F
In-Plane, Dry, 365° Oven Cured; ASTM D3518
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS 630-500 Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Shear Modulus 4.14 GPa

@Temperature 121 °C
600 ksi

@Temperature 250 °F
In-Plane, Wet, 365° Oven Cured; ASTM D3518
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS 630-500 Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Shear Modulus 4.14 GPa

@Temperature 71.1 °C
600 ksi

@Temperature 160 °F
In-Plane; Dry; ASTM D3518
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Shear Modulus 4.14 GPa

@Temperature 71.1 °C
600 ksi

@Temperature 160 °F
In-Plane; Wet; ASTM D3518
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..