Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.975 GPa @Temperature -20.0 °C |
286.5 ksi @Temperature -4.00 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |