Mechanical Properties Metric English Comments
Shear Modulus 1.83 GPa

@Temperature 20.0 °C
265 ksi

@Temperature 68.0 °F
DAM; ISO 6721
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Shear Modulus 1.83 GPa

@Temperature 20.0 °C
265 ksi

@Temperature 68.0 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..