Polymer Property : Shear Modulus = 218.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 1.509 GPa

@Temperature 0.000 °C
218.8 ksi

@Temperature 32.0 °F
Torsion Pendulum Method
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Shear Modulus 1.509 GPa

@Temperature 0.000 °C
218.8 ksi

@Temperature 32.0 °F
Torsion Pendulum Method
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Shear Modulus 1.509 GPa

@Temperature 0.000 °C
218.8 ksi

@Temperature 32.0 °F
Torsion Pendulum Method
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..