Shear Modulus 2.76 GPa

@Temperature 232 °C
400 ksi

@Temperature 450 °F
In-Plane, Dry; ASTM D790
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-..
Shear Modulus 2.76 GPa

@Temperature 163 °C
400 ksi

@Temperature 325 °F
In-Plane; Wet
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber
Information provided by HexCel