Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 2.393 GPa

@Temperature 10.0 °C
347.1 ksi

@Temperature 50.0 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 10B140 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66Minlon 10B140 NC010 is a 40% mineral reinforced polyamide 66 for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers