Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.199 GPa @Temperature -100 °C |
318.9 ksi @Temperature -148 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |