Mechanical Properties Metric English Comments
Shear Modulus 2.00 GPa

@Temperature 150 °C
290 ksi

@Temperature 302 °F
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..