Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.065 GPa @Temperature -50.0 °C |
154.5 ksi @Temperature -58.0 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |