Shear Modulus 1.0443 GPa

@Temperature -30.0 °C
151.47 ksi

@Temperature -22.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani..
Shear Modulus 1.0443 GPa

@Temperature -30.0 °C
151.47 ksi

@Temperature -22.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b..