Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.992 GPa @Temperature 20.0 °C |
144 ksi @Temperature 68.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Shear Modulus | 0.993 GPa @Temperature 150 °C |
144 ksi @Temperature 302 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G35HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL NC010 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |