Mechanical Properties Metric English Comments
Shear Modulus 0.907 GPa

@Temperature 20.0 °C
132 ksi

@Temperature 68.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr..