Polymer Property : Shear Modulus = 11740 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 80.94 GPa

@Temperature 25.6 °C
11740 ksi

@Temperature 78.0 °F
Cold Worked and Aged
Latrobe MP35N® Alloy
MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties - ultra high strength, toughness, ductility, and outstanding corrosion resistance. The ..