Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 73.8 GPa @Temperature 22.0 °C |
10700 ksi @Temperature 71.6 °F |
|
Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with ex.. |
|||
Shear Modulus | 74.0 GPa @Temperature 300 °C |
10700 ksi @Temperature 572 °F |
|
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor.. |
|||
Shear Modulus | 74.0 GPa @Temperature 22.0 °C |
10700 ksi @Temperature 71.6 °F |
|
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-.. |