Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 72.4 GPa @Temperature 100 °C |
10500 ksi @Temperature 212 °F |
|
Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with ex.. |