Polymer Property : Shear Modulus = 10200 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 70.0 GPa

@Temperature 427 °C
10200 ksi

@Temperature 801 °F
ATI Allegheny Ludlum AL 625HP™ Stainless Steel
Nickel-based superalloy. Characteristics:exceptional fatigue resistance, excellent resistance to oxidation and corrosion, outstanding strength and toughness over a range of temperatures from cryogen..