Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.166 GPa @Temperature -50.0 °C |
169.1 ksi @Temperature -58.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |