Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.812 GPa @Temperature 120 °C |
118 ksi @Temperature 248 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |