Shear Modulus 0.731 GPa

@Temperature 160 °C
106 ksi

@Temperature 320 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6  (Unverified Data**)
45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers