Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.578 GPa @Temperature 110 °C |
83.8 ksi @Temperature 230 °F |
DAM; ISO 6721 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |