Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.525 GPa @Temperature 160 °C |
76.1 ksi @Temperature 320 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR530L NC010 Polyethylene Terephthalate (PET) Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |